Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75, ASTM D648 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ASTM D648 |
Nilit Polynil® C50 PA66/6 Co-Polymer Description: NYLON 66/6 copolymerApplication: CompoundingInformation provided by NILIT. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/A |
PolyOne Bergamid™ B700 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ASTM D648 |
Resirene Resirene® 2220 Medium Impact Polystyrene Features:High FlowEasy ProcessingGood GlossHigh Tensile ModulusFDA Rating: 21 CFR 177.1640High ProductivityExternal LubricatedApplications:InjectionThin Wall ApplicationsHard to Fill MoldsHangersVid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75/Af |
Solvay TECHNYL® C 206 PA6, DRY Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75/Af |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RP004 is a compound based on PA66 resin containing PTFE, Silicone. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N802 PPE+HIPS (Asia Pacific) PPE/PS 80oC V2 FR high flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-93 |
Wellman Wellamid® FR1841-BK1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75 |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-93 |
Wellman Wellamid® GS40-60 42L-NBK1 40% Glass Sphere Reinforced Nylon 6 Description: Glass Sphere Reinforced Nylon 6Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 80.0 °C | >= 176 °F | DIN 53461 |
Polyram PlusTek RA102 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MR 409 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S170 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ASTM D648 |
E-Polymers TEKAMID® H14ST Super Toughness PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-2/AF |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ISO 75-2 |
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | ASTM D648 |
Chem Polymer Chemlon 104 Nylon 66, Medium Impact GP A medium viscosity, impact-modified, lubricated nylon 66 exhibiting improved toughness.Data provided by the manufacturer, Chem Polymer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 - 110 °C | 176 - 230 °F | GB/1634 |
Zhejiang Juner PC/PET Alloy Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | |
LATI Laticonther 75 GR/50 PBT, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |