Material Notes:
LNP* LUBRICOMP* RP004 is a compound based on PA66 resin containing PTFE, Silicone. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
5 mm/min; ISO 527
Elongation at Break 7.0 %
7.0 %
5 mm/min; ISO 527
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
Flexural Yield Strength 82.0 MPa
11900 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94