Material Notes:
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
chs 2 in/min; ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
Tangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
93.9 °C
201 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Vicat Softening Point 88.9 °C
192 °F
0.125 inch, 1 Kg; ASTM D1525