Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | ASTM D-648 |
Plaskolite Optix® CA - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | ASTM D648 |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C @Thickness 6.35 mm |
172 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C @Thickness 6.35 mm |
172 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ 81530 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 - 98.9 °C | 172 - 210 °F | Average value: 90.6 °C Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | ASTM D648 |
I. Stern GPPS-020 General Purpose Crystal Polystyrene Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 92RK Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Entec Hyrene® PS-HI 14/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | |
Aclo Accutech Polypropylene Copolymer CP0437G10CL Glass Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | |
Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | ASTM D648 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | |
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | ASTM D648 |
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 922 NAT Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.8 °C | 172 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |