Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO.75 DIN.53461 |
Omnia Plastica PE 500 - Polyethylene 500 Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C @Thickness 3.20 mm |
122 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
Ovation Polymers Nemcon™ E HDPE 11000 HDPE HDPE-ESD Range Conductivity with improved processability and UV resistance.Information provided by Ovation Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75/2Af |
Radici Radilon® CS38 Copolyamide 6 semiaromatic Film extrusion gradeInformation provided by Radici group. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | |
Radici Radilon® S USX200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | STN EN ISO 75/A |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 - 68.0 °C | 122 - 154 °F | Average value: 60.8 °C Grade Count:4 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75/Af |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
SCG Chemicals EL-Proâ„¢ P750J Polypropylene Injection Molding Key Characteristics:Excellent clarityHigh productivityGood processability and stiffnessHigh glossOdorlessSafe for food contactRecommended Applications:Food container, utensilMedical parts such as sy.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75 |
Unipetrol PP MONSTEN® GB 504 Polypropylene Impact Copolymer Made for injection molding applications. Slip and antiblocking agent stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-93 |
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy Description: Nylon/Polypropylene AlloyInformation provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1245 is a 20% CAC03 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | 120°C per hour; ISO 752 |
Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000/58 HWUVCP Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO 75-2/A |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | ISO R75 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | |
Arkema Group Rilsan® BMV Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | cond.; ISO 75 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |