Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® CS38 Copolyamide 6 semiaromatic

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Radici Radilon® CS38 Copolyamide 6 semiaromatic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Film extrusion gradeInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 4.0 %
4.0 %
ISO 524-1/2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1/2
Flexural Strength 65.0 MPa
9430 psi
ISO 178
Flexural Modulus 1.75 GPa
254 ksi
ISO 178
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 193 °C
379 °F
ISO 1135 7-1-3
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75/2Af
Vicat Softening Point 70.0 °C
158 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in