Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)
Information provided by Ravago
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C

@Thickness 3.20 mm
462 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66
LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66
LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific)
LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C

@Thickness 3.20 mm
462 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66
LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66
LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C

@Thickness 3.20 mm
462 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66
LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C

@Thickness 3.20 mm
462 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
80*10*4 s=60mm; ISO 75-1 a
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33H 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman SCHULAMID® 66 GF33 33% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b..
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
Ashley Polymers Ashlene® 520-13G Nylon 66, 13% Glass Reinforced
13% Glass reinforced Nylon 66.Data provided by the manufacturer
Deflection Temperature at 1.8 MPa (264 psi) 239 °C
462 °F
ASTM D648
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin