Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C @Thickness 6.40 mm |
442 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | ASTM D648 |
Covestro Petlon® 4835 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | ISO 75/Af |
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM AUT230 PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C @Thickness 3.20 mm |
442 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 (Asia Pacific) LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM AUT230 PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | ISO 75-1, 2 |
Polyplastics FR-PET® CN3030SD Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | ASTM D648 |
Plenco 50240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66 Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |