Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | |
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 33% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
Ravago Manufacturing Americas Enviramid™ N1335HL BK Post Consumer Recycle Nylon 66, 35% Glass Filled Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-1, -2 |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75/Af |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C @Thickness 3.20 mm |
437 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 (Asia Pacific) LNP* Thermocomp* RFB53XXZ is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Polyram PlusTek RA325G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced, Flame Retardant, Halogen Free 30% Glass-fiber reinforced, flame retardant halogen free Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-93 |
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK4015H 40% Glass Fiber/Mineral Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-1/-2 |
DSM Arnite® AV2 340 PET-20% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO 75 |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ISO R75 |
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuP.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | DIN 53461 |
Polyram Polytron A40B01 Nylon 66, 40% Long Fiber A 40% long fiber glass reinforced black nylon 6.6 heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind. |