Polyram Polytron A40B01 Nylon 66, 40% Long Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Polyram
Trade Name Polytron
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron A40B01 Nylon 66, 40% Long Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A 40% long fiber glass reinforced black nylon 6.6 heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 195 MPa
28300 psi
ASTM-D638
Elongation at Break 2.65 %
2.65 %
ASTM-D638
Tensile Modulus 10.65 GPa
1545 ksi
ASTM-D790
Flexural Strength 295 MPa
42800 psi
ASTM-D790
Flexural Modulus 10.7 GPa
1550 ksi
ASTM-D790
Izod Impact, Notched 2.20 J/cm

@Temperature 23.0 °C
4.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
DIN 53461