Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | ASTM D648 |
Niche Polymer PCABSN8BK PC/ABS Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East) GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Unannealed; ISO 75-2/A |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East) CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Unannealed; ISO 75-2/A |
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | |
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Annealed, 80°C, 4 hours; ISO 175 |
LG Chemical LG-709 ABS, Low Gloss, Super High Heat Resistance Information Provided by LG Chem |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | ASTM D648 |
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL EZ250 PPE+PS Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PX0844 PPE+PS PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | ASTM D 648 |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | ISO 75-1, 2 |
Polyplastics Duranex® H7500 Polybutylene Terephthalate (PBT), Low warpage DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C | 234 °F | ISO 75-1/-2 |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112 °C @Thickness 3.20 mm |
234 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |