Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | 120°C/h; ASTM D 648 |
Polimeri Europa Sinkral® E 332 ABS Resin Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hysun™ 678UV ASA Available in North America Additive: UV Stabilizer Features: Good Impact Resistance and High Heat ResistanceRoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP KONDUIT MT00E PP LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 6.40 mm |
217 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 218 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 218 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS E GM15 LE 15% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 218 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 1018121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C @Thickness 3.20 mm |
217 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | annealed; ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ASTM D648 |
CPC - Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated tempera.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | 0.25 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ASA T-105 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | unannealed; ISO 75 |
Chi Mei Polylac® PA-777D ABS - High Heat Super High Heat |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | Method A - Annealed; ASTM D-648 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ASTM D648 |
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |