Thermal Properties Metric English Comments
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East)
CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin..
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region.
Glow Wire Test 750 °C

@Thickness 1.60 mm
1380 °F

@Thickness 0.0630 in
Ignition Temperature; IEC 60695-2-13
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Glow Wire Test 750 °C

@Thickness 1.50 mm
1380 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers
Glow Wire Test 750 °C

@Thickness 1.50 mm
1380 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Glow Wire Test 750 °C

@Thickness 1.50 mm
1380 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 750 °C

@Diameter 3.00 mm
1380 °F

@Diameter 0.118 in
GWFI; IEC 60695-2-12
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
GWFI/GWT
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
GWFI/GWT
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
GWIT
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant
Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
GWIT
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
GWFI/GWT
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified
Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East)
VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Glow Wire Test 750 °C

@Thickness 1.00 mm
1380 °F

@Thickness 0.0394 in
GWIT; IEC 60695-2-13
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Glow Wire Test 750 °C

@Thickness 1.60 mm
1380 °F

@Thickness 0.0630 in
ISO 60695-2-12
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY
Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent ..
Glow Wire Test 750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
b.o. EDF HN60 E.02
Covestro Makrolon® 2607 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
b.o. EDF HN60 E.02
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epicarb PC BLACK IQ Polycarbonate
Characteristics: good fluidity, good impact, industrial quality
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact
Characteristics: high fluidity, high impact
Glow Wire Test 750 °C

@Thickness 3.20 mm
1380 °F

@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilon PC UVR Polycarbonate, High Impact
Characteristics: high fluidity, high impact, UV resistant
Glow Wire Test 750 °C

@Thickness 3.20 mm
1380 °F

@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
EPICHEM Epicarb PC Polycarbonate
Characteristics: high fluidity, good impact
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epicarb PC Polycarbonate
Characteristics: high fluidity, good impact
Glow Wire Test 750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Glow Wire Test 750 °C

@Thickness 3.00 mm
1380 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
Glow Wire Test 750 °C

@Thickness 0.750 mm
1380 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Glow Wire Test 750 °C

@Thickness 1.50 mm
1380 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Glow Wire Test 750 °C

@Thickness 0.750 mm
1380 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Glow Wire Test 750 °C

@Thickness 1.50 mm
1380 °F

@Thickness 0.0591 in
IEC 60695-2-12
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions...