Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 650 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 650 °C

@Thickness 1.00 mm
1200 °F

@Thickness 0.0394 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East)
Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by ..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 60695-2-12
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East)
CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
Glow Wire Test 650 °C

@Thickness 0.800 mm
1200 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
Ignition Temperature; ISO 60695-2-13
Solvay TECHNYL® A 208F PA66, DRY
Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta..
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
Ignition Temperature; ISO 60695-2-13
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
ISO 60695-2-12
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY
Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry..
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
ISO 60695-2-12
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is ..
Glow Wire Test 650 - 750 °C

@Thickness 3.20 mm
1200 - 1380 °F

@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS
Glow Wire Test 650 - 750 °C

@Thickness 2.00 mm
1200 - 1380 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber
Characteristics: 10% glass fibre filled
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber
Characteristics: 17% glass fibre filled
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
Glow-Wire Ignition; IEC 60695-2-13
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Glow Wire Test 650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
Glow Wire Flammability Index; IEC 60695-2-12
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 650 °C

@Thickness 1.50 mm
1200 °F

@Thickness 0.0591 in
IEC 60695-2-12
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Copyright © lookpolymers.com All Rights Reserved