Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=0.750 mm |
140 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.10 mm |
140 °F @Thickness >=0.0827 in |
|
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|