Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical with Impact = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 105 °C

@Thickness 0.750 mm
221 °F

@Thickness 0.0295 in
UL 746
PolyOne Maxxam™ FR PP FR 7B01 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
UL 746
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 105 °C

@Thickness >=2.50 mm
221 °F

@Thickness >=0.0984 in
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
UL RTI, Mechanical with Impact 105 °C

@Thickness >=2.50 mm
221 °F

@Thickness >=0.0984 in
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical with Impact 105 °C

@Thickness >=2.50 mm
221 °F

@Thickness >=0.0984 in
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical with Impact 105 °C

@Thickness >=1.50 mm
221 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
Description: LUPOY PC 1302EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 105 °C

@Thickness >=1.60 mm
221 °F

@Thickness >=0.0630 in
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin
Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 105 °C

@Thickness >=1.60 mm
221 °F

@Thickness >=0.0630 in
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin
Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 105 °C

@Thickness >=1.50 mm
221 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1303-10 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical with Impact 105 °C

@Thickness >=1.50 mm
221 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin
Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 105 °C

@Thickness 0.800 mm
221 °F

@Thickness 0.0315 in
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
UL RTI, Mechanical with Impact 105 °C

@Thickness 0.750 mm
221 °F

@Thickness 0.0295 in
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
UL RTI, Mechanical with Impact 105 °C

@Thickness 0.810 mm
221 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.50 mm
221 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
UL RTI, Mechanical with Impact 105 °C

@Thickness 0.860 mm
221 °F

@Thickness 0.0339 in
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded
Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.60 mm
221 °F

@Thickness 0.0630 in
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
UL RTI, Mechanical with Impact 105 °C

@Thickness 1.60 mm
221 °F

@Thickness 0.0630 in
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded
Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
UL RTI, Mechanical with Impact 105 °C

@Thickness 3.00 mm
221 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..