Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 105 °C @Temperature 105 °C |
221 °F @Temperature 221 °F |
UL 746 |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC810FE PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810FE is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ferrite colour effects. The colour package may effect performance.This data was supp.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | Ul746B |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl.. |
|||
UL RTI, Mechanical without Impact | 105 - 105 °C @Temperature 105 - 105 °C |
221 - 221 °F @Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL746B |
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | |
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Ultem CRS5211 PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5301 PEI 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East) LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific) High heat PPO/HIPS alloy suitable for use in some potable water applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |