Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.860 mm |
284 °F @Thickness 0.0339 in |
UL 746B |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific) Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® HR426 PBT AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5722 10% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5723 15% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5726 30% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL 746B |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry) Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
UL RTI, Electrical | 140 °C @Thickness 0.810 mm |
284 °F @Thickness 0.0319 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Electrical | 140 °C | 284 °F | UL746B |
PlastxWorld CEVIAN® B5523 15% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
UL RTI, Electrical | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
BASF Ultramid® B3UG4 LS Grey22985 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |