PlastxWorld CEVIAN® B5722 10% GF PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B5722 10% GF PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.3 MPa
10200 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Flexural Yield Strength 119 MPa
17200 psi
ASTM D790
Flexural Modulus 4.81 GPa
697 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
0.25 inch; ASTM D648
UL RTI, Electrical 140 °C
284 °F
UL746B
UL RTI, Mechanical with Impact 100 °C
212 °F
UL746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in