Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3413HF PC (Asia Pacific) 30% glass reinforced, high flow PC. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL2003 PC Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
UL RTI, Electrical | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3010-22 Polycarbonate Resin Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 0.750 - 0.800 mm |
176 °F @Thickness 0.0295 - 0.0315 in |
|
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Electrical | 80.0 °C @Thickness 0.750 - 0.800 mm |
176 °F @Thickness 0.0295 - 0.0315 in |
|
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
UL RTI, Electrical | 80.0 °C @Thickness >=0.700 mm |
176 °F @Thickness >=0.0276 in |
|
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin Polycarbonate-resin-base flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even at a thinner th.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific) Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
|
Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® XT5010 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Easy processing• Low.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 4502 Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 5.99 mm |
176 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |