Polymer Property : UL RTI, Electrical = 110 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Lexan® FL920 PC (Europe-Africa-Middle East)
LEXAN FL920 is a foamable grade of LEXAN polycarbonate, containing 20% glass-fibre is designed of applications where superior flexural and tensile charasterics are required. LEXAN FL920 also offers ..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Lexan® FL930 PC
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
UL RTI, Electrical 110 °C
230 °F
UL746B
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
UL RTI, Electrical 110 °C
230 °F
UL746B
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications.
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
UL RTI, Electrical 110 °C
230 °F
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406P PPE
NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific)
10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific)
GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific)
PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific)
Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH5120 PPE+PS
Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific)
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL EN265 PPE+PS
Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated.
UL RTI, Electrical 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific)
Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad..
UL RTI, Electrical 110 °C
230 °F
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding
Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
UL RTI, Electrical 110 °C
230 °F
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized
UL RTI, Electrical 110 °C
230 °F
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized