| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech Polycarbonate POL051G20L Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 100 MPa | 14500 psi | ASTM D638 |
| Tensile Strength, Yield | 102.0 MPa | 14790 psi | ASTM D638 |
| Elongation at Break | 7.0 % | 7.0 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 4.100 GPa | 594.6 ksi | ASTM D638 |
| Flexural Strength | 170.0 MPa | 24650 psi | ASTM D790 |
| Flexural Modulus | 5.999 GPa | 870.1 ksi | ASTM D790 |
| Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F |