Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® CE2055 NC010 PBT
(Unverified Data**) Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C @Thickness 3.20 mm |
363 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C @Thickness 3.20 mm |
363 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C @Thickness 3.20 mm |
363 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | |
Covestro Apec® HT KU 1-9357/2 High-Heat Polycarbonate, 20% Glass Fiber Only opaque colors available, with 20% glass fiber reinforcement, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | |
Covestro Apec® HT KU 1-9363 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Perf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | ASTM D648 |
A. Schulman ComAlloy Lubrilon® 62S1 Internally Lubricated, Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | ASTM D648 |
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer Information provided by Advanced Laser Materials (ALM). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 °C | 363 °F | ASTM D648 |
ALM PA 860 White Nylon 11 SLS Prototyping Polymer Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 184 - 223 °C | 363 - 433 °F | Average value: 214 °C Grade Count:39 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |