Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75-1 |
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ASTM D648 |
SABIC PP 575P Polypropylene Homopolymer for Injection Molding Product Description: PP 575P is specially developed for producing rigid injection molding articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYasa 1614F UV-resistant ASA Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C @Thickness 6.40 mm |
208 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C @Thickness 3.20 mm |
208 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C @Thickness 3.20 mm |
208 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ASTM D648 |
Reliance Industries Repol H080EG Polypropylene REPOL Polypropylene H080EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Annealed, 80°C, 4 hours; ISO 75 |
LG Chemical AF-348 ABS, Flame Retardant, Heat Resistant, Weather Resistant Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | Annealed, 80°C, 4 hours; ISO 75 |
LG Chemical SH-610 ABS, Extrusion, High Impact Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ASTM D648 |
IRPC Polimaxx Polene 2300K Polypropylene Block Copolymer CHARACTERISTICS: HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR FURNITURE, HOUSEWARES, CLOSURES, CONTAINERS, AUTOPARTS AND ELECTRICAL APPLIANCES |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C @Thickness 3.20 mm |
208 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C @Thickness 6.40 mm |
208 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75 |
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | |
Styrolution NOVODUR® P2HE ABS, Extrusion Grade Extrusion grade, high gloss.Applications: Extruded sheets requiring medium property levels, profiles, blow molding parts. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75-2 |
Borealis BE375MO Polypropylene Copolymer BE375MO is a heterophasic copolymer. This grade is characterized by optimum combination of high impact strength and stiffness. This grade is formulated for an excellent antistatic performance. Elect.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | ISO 75-2 |
Borealis Daplen™ ED213AE TPO Compound Daplen ED213AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen ED213AE is a material with excellent impact/ stiffness ratio. Thanks to its low.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | DAM; ASTM D648 |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accucomp ABS ABS892BL High Heat Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech ABS ABS833G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437T20L1 Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 97.8 °C | 208 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L1 Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 98.0 °C | 208 °F | |
Polimeri Europa SINKRAL C443 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-25-20 Medium heat injection moulding grade. The availability of different industrial processes to manufa.. |