Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 94.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycolac® EX75 ABS
Multi-purpose, extrusion ABS providing a favorable balance of engineering properties.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycolac® INPBMAT ABS
Cross-linked SAN in styrenic matrix. Provides excellent gloss reduction properties. Maintains original polymer properties such as impact etc. Compatible with various polymer such as PVC and ABS. C..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East)
High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.18 mm
201 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Edgetek® XT X XT 1001 Natural Copolyester
Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Annealed; ISO 75-2A
Total Lacqrene® 3351(EU) Impact Polystyrene  (discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 12.7 mm
201 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Ineos ABS Lustran® 266 Specialty, Transparent  (discontinued **)
A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 3.20 mm
201 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC
LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Eastman Tenite 358-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Load not specified; ASTM D648
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Load not specified; ASTM D648
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS
LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75
Teijin Multilon TN-7000 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It is a typical type with high flowability, light resistance and heat stability that is suitable for a business machine ..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Unannealed; ISO 75-2/B
Samsung Cheil Industries Infino® PCA-NH1015V Flame Retardant
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 6.40 mm
201 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced
Anti-staticInformation provided by Samsung Cheil Industries.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 9450P ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75-2
Borealis HF700SA Polypropylene
HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75-2
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Eastman Tritan MX730 Copolyester
Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Eastman Tritan MX731 Copolyester
Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ISO 75
Ecomass® 706BI76 Filled ABS, Injection Molding Grade
Moderate Specific Gravity, Filled ABS, Plating Grade, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to traditional materialsInformation provided by Technical Polyme..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications
Product Description: A homopolymer resin based on Exxpol™ metallocene technology designed for medical, electronics and other applications requiring cleanliness. It provides lower, volatiles and ext..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
0.125";; ASTM D648
Diamond Polymers DIAMALOY GLY 9020 Sheet Extrusion Grade
Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, an..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
120°C/hr; ASTM D 648
Cossa Polimeri ESTABIO PL 0560 T10 Biodegradable Plastic
Biodegradable plastic for the extrusion of disposablesCertified for food contactInformation provided by Cossa Polimeri S.r.l.
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Carmel Olefins CAPILENE® E 50 E Polypropylene Homopolymer
CAPILENE® E 50 E is a low melt flow rate polypropylene homopolymer intended for extrusion, thermoforming and blow molding featuring very good process ability and melt stability. Products manufactur..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Braskem H 306 Injection Molding Polypropylene
Description: H 306 is a medium melt flow rate additivated homopolymer used for general purposes. It suitable for injection moulding and fiber extrusion. This product exhibits excellent processabilit..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 - 150 °C
201 - 302 °F
Average value: 128 °C Grade Count:140
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Unannealed; ASTM Data
Styron Magnum™ 9020 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
Polimeri Europa KOBLEND PCA 51 PC+ABS  (discontinued **)
Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 90°C Main application field..
Copyright © lookpolymers.com All Rights Reserved