Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C @Thickness 6.35 mm |
185 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CH042L Polypropylene, Homopolymer, Straw and Extrusion, Antistat COPYLENE™ CH042L is specifically designed for application in extrusion applications such as straws. Applications: Straws.Information provided by Phillips 66. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Ineos H02G-00 Polypropylene Homopolymer This is a low melt flow rate general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of sheet, film, and profile extrusion applic.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-8302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8302 is developed for extru.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C @Thickness 6.40 mm |
185 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Spartech PP7230 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East) NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C @Thickness 3.20 mm |
185 °F @Thickness 0.126 in |
ASTM D648 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
A. Schulman PP 1692 Polypropylene High Impact Copolymer DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Entec Hypro™ PP-CP10/10 Impact Copolymer, 10 Melt Flow This product is intended for injection molding applications such as automotive, appliance, lawn and garden, consumer products and industrial application. This product offers high impact properties a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | |
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | |
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | |
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | ASTM D648 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | |
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | Unannealed; ISO 75B-1, -2 |
LyondellBasell Hifax™ HSBMCB1158LS Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impa.. |