Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose
(discontinued **) General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Asahi Kasei Tenac®-C 7510 Acetal Copolymer, High Flow
(discontinued **) High-flow grade, suited for thin-wall, long-flow-distance moldings.Applications: Lighters, aerosol bottles, fasteners.This product is not a part of the standard product line dated 2003. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® K900 Standard Grade Acetal Resin Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® WR701 Wear Modified Acetal Resin Improved weather resistant and easy flow grade. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | Unannealed; ASTM D648 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
IRPC Polimaxx Polene 2311LCX GA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% GLASS FIBRE REINFORCED, HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS, LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOP.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East) PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648B |
Teknor Apex Synres® PP G30 19 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)
(Unverified Data**) Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | DAM; ASTM D648 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Aclo Accucomp Polyacetal (POM) ACE092L Medium Viscosity |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ashley Polymers Ashlene® 190 Acetal A general purpose, medium viscosity, natural.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ashley Polymers Ashlene® R195B Acetal A general purpose, low viscosity with excellent toughness, strength, stiffness, lubricity in black. Available in UV stabilized grades: R195-B2 (good weatherability); R195-HB2 (maximum weatherabili.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Cheng Yu Plastic FV30710 POM, 10% Mineral Reinforced |