Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | ASTM D648 |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 3.18 mm |
306 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPC-20G Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 3.18 mm |
306 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PPH-10G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 - 165 °C | 306 - 329 °F | Average value: 161 °C Grade Count:16 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 3.20 mm |
306 °F @Thickness 0.126 in |
ASTM D648 |
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 4.00 mm |
306 °F @Thickness 0.157 in |
after annealing 150°C 16 hr; ASTM D648 |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
Fiberfil® J-61/10 Polypropylene Copolymer, 10% Glass Fiber Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 3.20 mm |
306 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PC GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PC GF20 X 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Mold ReleaseFeatures: Good Mold Release and High FlowInformation provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | HDT-A; ISO 75-2 |
Borealis Xmod™ GB305HP High Performance 35% Glass Fiber Reinforced Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | ASTM D648 |
Tipco Tipcolene® SEB 300 - 30% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 30% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | HDT-A; ISO 75-2 |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | ASTM D648 |
Clariant Renol PP1100N40CC Polypropylene Homopolymer, 40% Glass Fiber and Mineral Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-0738 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-25FG-1734 25% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
Adell DR-18 40% Glass Reinforced Polycarbonate |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C @Thickness 6.35 mm |
306 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 305 °F | ASTM D648 |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |