Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Hyosung Topilene S905 PP S905 Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C @Thickness 6.40 mm |
230 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1,-2 |
Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
LG Chemical SEETEC H1500 Polypropylene Homopolymer Features: SEETEC H1500 is a high flow homopolymer suitable for injection molding applications. SEETEC H1500 exhibits a high flowability combined with a good mechanical property balance. SEETEC H1500.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Spartech PP7140 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON MD000I PP (Europe-Africa-Middle East) LNP* Stat-kon* MD000I is a compound based on Polypropylene resin. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C @Thickness 6.40 mm |
230 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® 1102 PBT+PC Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
SPS Guang Zhou SAMATâ„¢ 666(f1) Flame-retarded Polypropylene Characteristic: Flame retardance, weather resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C @Thickness 3.20 mm |
230 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1/-2 |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | Unannealed; ASTM D648 |
Dow 500.00 Developmental Performance Polypropylene Polymer D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336C40L Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Cheng Yu Plastic BK1022 Electric Conducting Polypropylene, Injection |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | |
BASF Procom® D 1133 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Ashley Polymers Ashlene® 830SMS Nylon 6, MoS2 Filled Basic Nylon 6, medium viscosity, lubricated with Molybdenum Disulfide.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
Tipco Tipcolene® HR 7224 - 25% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer 25% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive DashboardProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC TS15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |