| Category | Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced |
| Manufacturer | Ineos ABS |
| Trade Name | Lustran® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Transverse | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
| Melt Flow | 6.5 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
6.5 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | 1.7 % | 1.7 % | 50 mm/min; ISO 527-1,-2 |
| Tensile Modulus | 8.00 GPa | 1160 ksi | 1 mm/min; ISO 527-1,-2 |
| Flexural Strength | 162 MPa | 23500 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-1,-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ISO 75-1,-2 |
| Vicat Softening Point | 108 °C <br>@Load 5.10 kg |
226 °F <br>@Load 11.2 lb |
50°C/hour; ISO 306 |
| Flammability, UL94 | HB <br>@Thickness 1.60 mm |
HB <br>@Thickness 0.0630 in |