Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Triax® DP 3155 ABS + Polyamide Blend (DAM)
(discontinued **) Key Features:Contains FillerSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance, good surface, good flowability (Easy Flow), low warpage |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SILTEM-STM1500 PEI (Europe-Africa-Middle East) SILTEM STM1500 is a flexible siloxane-polyetherimide copolymer for cable and wire coatings. RoHS compliant. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX GTX976 PPE+PA (Europe-Africa-Middle East) NORYL GTX976 is a material especially designed for electrostatic painting and powder coating applications. This material combines high impact performance with conductivity in an unique way.This data.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 3300H Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T45 PG Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4073 nat PA610 Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materi.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makroblend® UT5205 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 90 LXS PAMACM12 Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |