Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 3.18 mm |
162 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM-D648 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |