Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
Manufacturer | PolyOne Corporation |
Trade Name | Geon™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
Spiral Flow | 61.0 cm | 24.0 in |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 80 | 80 | ASTM D2240 |
Tensile Strength, Yield | 48.3 MPa | 7010 psi | 51 mm/min; ASTM D638 |
Elongation at Break | 44 % | 44 % | 51 mm/min; ASTM D638 |
Tensile Modulus | 2.79 GPa | 405 ksi | 51 mm/min; ASTM D638 |
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
Izod Impact, Notched | 5.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
9.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
75.0 °C @Thickness 6.35 mm |
167 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 68.9 °C @Thickness 6.35 mm |
156 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Annealed; ASTM D648 | |
Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
ALL; UL 94 |
5VA @Thickness 1.50 mm |
5VA @Thickness 0.0591 in |
ALL; UL 94 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 199 - 210 °C | 390 - 410 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Features | General Purpose | |
Medium Flow | ||
Medium Impact Resistance | ||
Forms | Pellets | |
Generic Material | PVC, Rigid | |
Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
RoHS Compliance | RoHS Compliant | |
Uses | Construction Applications | |
General Purpose | ||
Outdoor Applications |