| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 76 | 76 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 32.9 MPa | 4770 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 4.25 GPa | 616 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 69.6 MPa | 10100 psi | ASTM D790 |
| Flexural Modulus | 4.08 GPa | 592 ksi | ASTM D790 |
| Dart Drop Total Energy | 20.5 J/cm @Temperature 23.0 °C |
0.0384 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| 20.5 J/cm @Temperature 23.0 °C |
0.0384 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 78.9 °C @Thickness 3.18 mm |
174 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| 80.0 °C @Thickness 3.18 mm |
176 °F @Thickness 0.125 in |
Annealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 3.18 mm |
162 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
| 78.9 °C @Thickness 3.18 mm |
174 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 188 °C | 360 - 370 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Colors Available | |
| Forms | Cube | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Vertical Blinds |