Polymer Property : Glass Transition Temp, Tg = 143 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 143 - 150 °C
289 - 302 °F
Average value: 145 °C Grade Count:5
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 150P Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 450PF Fine Powder Grade
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia..
Glass Transition Temp, Tg >= 143 °C
>= 289 °F
Onset; ISO 11357
Victrex® PEEK 650P PolyEtherEtherKetone
High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Glass Transition Temp, Tg 143 °C
289 °F
ISO 11357
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Glass Transition Temp, Tg 143 °C
289 °F
DSC
Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating
VICOTE 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for low..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Glass Transition Temp, Tg 143 °C
289 °F
Covestro Makrolon® DP 1-1265 Polycarbonate, Injection Grade  (discontinued **)
Injection molding grade with exceptionally good flow, for Digital Versatile Discs (DVD).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha..
Glass Transition Temp, Tg 143 °C
289 °F
Zeus PEEK Tubing
PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used..
Glass Transition Temp, Tg 143 °C
289 °F
After 1 hr at 120°C DSC 20°C/min
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix
HexPly® M47 is a toughened, self extinguishing 140ºC curing epoxy resin matrix that has been developed for the performance car market. It exhibits good strength retention at elevated temperature, ..
Glass Transition Temp, Tg 143 °C
289 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Glass Transition Temp, Tg 143 °C
289 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Glass Transition Temp, Tg 143 °C
289 °F
DIN 53 765
Ensinger Tecapeek® ID Metal Detectable Polyetheretherketone
Tecapeek™ ID metal detectable polyetheretherketone, made from Victrex® PEEK 450G polymer, is formulated to reduce the risk of product contamination and allow for easy detection of fragments in the..
Glass Transition Temp, Tg 143 °C
289 °F
dynamic; DIN 53 736
Hippe PEEK Polyetheretherketone
PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh..
Glass Transition Temp, Tg 143 °C
289 °F
ISO 11357-1
Murtfeldt Murpec® SP Polyetheretherketone
Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• ..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 380P Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 650G Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
Glass Transition Temp, Tg >= 143 °C
>= 289 °F
Onset; ISO 11357
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..
Glass Transition Temp, Tg 143 °C
289 °F
DSC
Victrex® Vicote® 703 Polyetheretherketone (PEEK) Powder
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail..
Glass Transition Temp, Tg 143 °C
289 °F
DSC
Victrex® Vicote® 704 Polyetheretherketone (PEEK) Powder
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, ..