Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® 704 Polyetheretherketone (PEEK) Powder

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® 704 Polyetheretherketone (PEEK) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, electronics or pharmaceutical parts. VICOTE Coatings can be applied using electrostatic or conventional dispersion spray techniques.The main ingredient of VICOTE Coatings is VICTREX® PEEK polymer, a linear, aromatic, semi-crystalline thermoplastic, widely regarded as one of the highest performing thermoplastic materials in the world. It offers a unique combination of properties to help processors and end users reach new levels of cost savings, performance, and product differentiation.Used in formulation of liquid dispersions.All information provided by Victrex.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Glass Transition Temp, Tg 143 °C
289 °F
DSC
UL RTI, Electrical 260 °C
500 °F
UL746B
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Konig Hardness 200 seconds
BS EN ISO 1522