Victrex® PEEK 380P Polyetheretherketone, Unreinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Victrex
Trade Name PEEK
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Victrex® PEEK 380P Polyetheretherketone, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compliant, colour natural.Information Provided by VICTREX®
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Viscosity 380000 cP
380000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa

@Temperature 23.0 °C
14500 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 3.70 GPa

@Temperature 23.0 °C
537 ksi

@Temperature 73.4 °F
ISO 527
Flexural Strength 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 178
Flexural Modulus 4.10 GPa

@Temperature 23.0 °C
595 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 0.550 kJ/m²

@Temperature 23.0 °C
0.262 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in