Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.335 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer
Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer
Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
DSC
Eastman Heatwave CF746 Polymer  (discontinued **)
Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 ..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
Eastman Vitiva PC715 PET  (discontinued **)
Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman Aqua 18696 PET  (discontinued **)
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman 7352 PET  (discontinued **)
VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman 9663 PET  (discontinued **)
VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
Eastman CB11E PET  (discontinued **)
VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
Eastman CB12 PET  (discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
DSC
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Goodfellow Cellophane, Rayophane Regenerated Cellulose Fiber
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
Specific Heat Capacity 1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
IEC 1006
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved