Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 50BW Nylon 66, General Purpose

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ascend Performance Materials Vydyne® 50BW Nylon 66, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 50BW is a general-purpose PA66 resin. Offered in natural and designed for extrusion-compounding applications, this product is available at two moisture levels: 0.2% (max) as Vydyne 50BW and 0.5% (max) as Vydyne 50BWFS. Vydyne 50BW provides the chemical resistance typical of PA66 to many chemicals, machine and motor oils, solvents and gasoline. Vydyne 50BW exhibits good initial color and color retention after compounding. Typical Applications/End Uses: CompoundingAvailability:Asia PacificEuropeNorth AmericaFeatures:Gasoline ResistanceGeneral PurposeGood Chemical ResistanceGood Color StabilityOil ResistantSolvent ResistantUses:CompoundingGeneral PurposeAppearance: Natural ColorForms: PelletsProcessing Method: Compounding and Compounding ExtrusionInformation provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Bulk Density 0.675 g/cc
0.0244 lb/in³
ASTM D1895
Relative Viscosity 45 - 51 cP
45 - 51 cP
ASDTM D789
Viscosity Measurement 137 - 148
137 - 148
sulfuric acid; ISO 307
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357
Optical Properties Metric English Comments
Yellow Index -4.00 %
-4.00 %
ASTM D1925
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
ASTM D789
Descriptive Properties Value Comments
RV, Formic Acid, ASTM D789 45-51