Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 190 °C | 374 °F | |
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high.. |
|||
Melting Point | 190 °C | 374 °F | crystalline melting point; ASTM D4591 |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Melting Point | 190 °C | 374 °F | crystalline melting point; ASTM D4591 |
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Melting Point | 190 °C | 374 °F | crystalline melting point; ASTM D4591 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Melting Point | 190 °C | 374 °F | crystalline melting point; ASTM D4591 |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Melting Point | 190 - 200 °C | 374 - 392 °F | Huntsman/TMA |
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 190 °C | 374 °F | Peak |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 190 °C | 374 °F | Peak |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 190 °C | 374 °F | DIN EN ISO 314 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Melting Point | 190 °C | 374 °F | DIN 53736 |
Isoflon PSU Polysulfone Electrical insulating productsRigidHigh chemical, fire and temperature resistanceInformation provided by Isoflon. |
|||
Melting Point | 190 - 200 °C | 374 - 392 °F | MQSA 111 |
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance.. |
|||
Melting Point | 190 - 200 °C | 374 - 392 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® ECO D12T85 Thermoplastic Polyurethane Pearlthane® ECO D12T85 is a 85 Shore A, High Performance natural TPU based on Renewable Sources with ca. 46% renewable content according to ASTM D6866 for Injection Moulding applications. This na.. |
|||
Melting Point | 190 - 200 °C | 374 - 392 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application.. |
|||
Melting Point | 190 °C | 374 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 190 °C | 374 °F | ISO 11357-1/-2 |
Suzhou Hipro Polymers Hiprolon® 400 NN Nylon, conditioned Hiprolon® 400 NN is a medium viscosity specialty polyamide. Features: low density, low water absorption, high dimension stability, high notched impact resistance in large temperature ranges, and.. |
|||
Melting Point | 190 °C | 374 °F | |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Melting Point | 190 °C | 374 °F | ISO 3146 |
Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as se.. |
|||
Melting Point | 190 °C | 374 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Melting Point | <= 190 °C | <= 374 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |
|||
Melting Point | 190 °C | 374 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
Melting Point | 190 °C | 374 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Melting Point | 190 °C | 374 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f.. |
|||
Melting Point | 190 °C | 374 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f.. |
|||
Melting Point | 190 °C | 374 °F | 10 K/min |
BASF Ultramid® C40 01 PA66/6 (Dry) Ultramid C40 01 is a high viscosity, copolymer PA6/66 grade. Its very low melting point compared to standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It c.. |
|||
Melting Point | 190 °C | 374 °F | 10 K/min |
BASF Ultramid® C40LX 01 PA66/6 (Conditioned) Ultramid C40LX 01 is a high viscosity, copolymer PA6/66 grade. Improved transparency and gloss are enhanced by the incorporation of a high dose of lubricant. It conforms to FDA requirements includ.. |
|||
Melting Point | 190 °C | 374 °F | 10 K/min |
BASF Ultramid® C40LX 01 PA66/6 (Dry) Ultramid C40LX 01 is a high viscosity, copolymer PA6/66 grade. Improved transparency and gloss are enhanced by the incorporation of a high dose of lubricant. It conforms to FDA requirements includ.. |
|||
Melting Point | 190 °C | 374 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Melting Point | 190 °C | 374 °F | Average value: 190 °C Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Melting Point | 190 - 238 °C | 374 - 460 °F | Average value: 219 °C Grade Count:60 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |