Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Melting Point | 96.0 °C | 205 °F | Exxon Method |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3418 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 96.0 °C | 205 °F | |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Melting Point | 96.0 - 135 °C | 205 - 275 °F | |
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 137 °C | 205 - 279 °F | |
Indium Corp. Indalloy 81 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 - 139 °C | 205 - 282 °F | |
Indium Corp. Indalloy 83 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 °C | 205 °F | Eutectic |
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 96.0 - 107 °C | 205 - 225 °F | |
Indium Corp. Indalloy 49 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 96.0 °C | 205 °F | DSC |
Silon Tabond 2005 Adhesive Resin TABOND 2005 is a plastomer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass .. |
|||
Melting Point | 96.0 °C | 205 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 96.0 °C | 205 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Melting Point | 96.0 °C | 205 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3417- ISO 3146 |
DuPont Elvax® 770 Ethylene Vinyl Acetate DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application.. |
|||
Melting Point | 96.0 °C | 205 °F | ASTM D3417- ISO 3146 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Melting Point | 96.0 °C | 205 °F | TRN-14 |
Tipco Tipcolite® TPF 1115 - Unreinforced Thermoset Phenolic Resin, 43 mm Norton Flow with 9% Hexamine Unreinforced Phenolic Resin having 43mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Melting Point | 96.0 °C | 205 °F | DSC; ASTM D3418 |
Westlake Tymax™ GA7501 Anhydride Modified Acrylate Copolymer (Developmental) Westlake GA7501 is an anhydride modified acrylate copolymer for extrusion coating and cast film tie-layers. This resin is designed to function as a coextruded tie-layer in multilayer applications wh.. |
|||
Melting Point | 96.0 °C | 205 °F | DTA |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 96.0 °C | 205 °F | Dow Method (DSC) |
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP) AFFINITY™ PF 1140G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to be used in a variety of demanding applications including form-fill-seal packaging and fre.. |
|||
Melting Point | 96.0 °C | 205 °F | Dow Method |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2910 M Q 47 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Ethylene/Acrylate Copolymer Used in the manufacture of economical composite films of Lucalen and PE-LD, and as a primer for aluminum steel composites.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2920 M Q 225 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | 10°C/min |
Arkema Group Evatane® 1090 VN 3 Ethylene Vinyl Acetate Description: EVA copolymer made by high pressure tubular process.Applications:Grade for molding flexible articles.Examples: Closures, plugs, swimming flippers, toys.ISO data provided by the manufact.. |
|||
Melting Point | 96.0 °C | 205 °F | |
BASF Lucalen® A 2910 M Ethylene/Acrylate Copolymer For coating metals such as aluminum and steel, and as a primer for composites of metal or paper with Lupolen. Contains an antioxidant.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 96.0 °C | 205 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 96.0 °C | 205 °F | Eutectic |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |