Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 90.0 °C | 194 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 90.0 °C | 194 °F | Exxon Method |
ExxonMobil Escorene® LD-706 High EVA Cast Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.3% vinyl acetate copolymer film resin designed for coextruded cast film applications.Applications: Coextruded meat packaging film; Sealant in c.. |
|||
Melting Point | 90.0 - 105 °C | 194 - 221 °F | |
Kazanorgsintez NMPE-3 Low-Molecular Polyethylene Notes: Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as compon.. |
|||
Melting Point | >= 90.0 °C | >= 194 °F | |
Hong Kun Group UV 783 UV Absorber CAS No. 76024-18-19 & 65447-77-0All information provided by Hongkun Group |
|||
Melting Point | 90.0 - 120 °C | 194 - 248 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-201 TPU-Polyester Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 90.0 °C | 194 °F | fusing temperature |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Melting Point | 90.0 °C | 194 °F | fusing temperature |
ICO Polymers ICOTEXâ„¢ 520-5076 500 Micron EVA Powder Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility,.. |
|||
Melting Point | 90.0 - 94.0 °C | 194 - 201 °F | |
Indium Corp. Indalloy 37 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 90.0 - 110 °C | 194 - 230 °F | |
LG Chemical LUTENE XL2808BK PE Compound Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically .. |
|||
Melting Point | 90.0 - 95.0 °C | 194 - 203 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Melting Point | 90.0 °C | 194 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 90.0 °C | 194 °F | |
Mitsui EXCEREXâ„¢ 48070B(T) Polymer Processing Aid EXCEREXâ„¢ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREXâ„¢ gains in a number of ares simultaneously, including faster processing speeds.. |
|||
Melting Point | 90.0 °C | 194 °F | ASTM D3418 |
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Melting Point | 90.0 °C | 194 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melting Point | 90.0 °C | 194 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Melting Point | 90.0 °C | 194 °F | DSC Peak; D3418 |
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF524 is an ethylene vinyl acetate copolymer with 14.5% VA. EF524 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Melting Point | 90.0 °C | 194 °F | ISO 11357 |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |
|||
Melting Point | 90.0 °C | 194 °F | Exxon Method |
ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications Product Description: Exact 3027 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3027 is designed for both monolayer and multilayer coe.. |
|||
Melting Point | 90.0 °C | 194 °F | ASTM D3418, ISO 3146 |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Melting Point | 90.0 °C | 194 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvaloy® AC34035 Ethylene Methyl Acrylate Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A.. |
|||
Melting Point | 90.0 °C | 194 °F | Tm |
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber Description: This crystalline ethylene-propylene-diene terpolymer (EPDM) has a low viscosity for excellent flow characteristics and hot green strength. It has been designed for property modification.. |
|||
Melting Point | 90.0 °C | 194 °F | ASTM-D3418 |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |
|||
Melting Point | 90.0 °C | 194 °F | 10°C/min |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Melting Point | 90.0 °C | 194 °F | ASTM D3417, ISO 3146 |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Melting Point | 90.0 °C | 194 °F | DTA |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 90.0 °C | 194 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® PE3507-2 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® PE3507-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applic.. |
|||
Melting Point | 90.0 °C | 194 °F | By DSC; ASTM D3418 - ISO 3146 |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Melting Point | 90.0 °C | 194 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |