Thermal Properties Metric English Comments
Melting Point 102 - 110 °C
216 - 230 °F
Pau Tai Lead stearate, Monomer Stabilizer
Stabilizer with low price, excellent lubricity with cadmium, barium.Applications: Rigid plate, injection soft products.
Melting Point 103 - 110 °C
217 - 230 °F
Pau Tai Cadmium stearate, Monomer Stabilizer
Transparent heat resistance stabilizer. Excellent effect if used with barium and tin series stabilizer. Excellent lubricant at high temperature operation.Applications: Rigid processing, adhesive pla..
Melting Point -7.78 - 110 °C
18.0 - 230 °F
Average value: 94.2 °C Grade Count:147
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Melting Point 80.0 - 110 °C
176 - 230 °F
TMA Melt Range
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
Melting Point 80.0 - 110 °C
176 - 230 °F
TMA Melt Range
Huntsman IROGRAN® CA116-205 TPU-Polyester
Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee..
Melting Point 100 - 110 °C
212 - 230 °F
Fine Organics FINAWAX HC Lubricant Additive
Applications: Distilled hydrocarbon wax as a strong external lubricant for rigid PVC extruded products, lubricant for cable compounds.Information provided by Fine Organics
Melting Point 90.0 - 110 °C
194 - 230 °F
LG Chemical LUTENE XL2808BK PE Compound
Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically ..
Melting Point 100 - 110 °C
212 - 230 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Pearlbondâ„¢ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ..
Melting Point 100 - 110 °C
212 - 230 °F
Fine Organics FINALUX GT 23 Composite Lubricant
Applications: One pack lubricant specially suggested for RPVC pressure pipes and commercial pipes, suitable for single as well as twin screw extruders.Information provided by Fine Organics
Melting Point 95.0 - 110 °C
203 - 230 °F
Goodfellow Roses Metal (Bi, Pb, Sn) Alloy
Fusible alloy. Uses include anchoring, mold applications and fusible links.Information provided by Goodfellow.
Copyright © lookpolymers.com All Rights Reserved