Material Notes:
Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically developed to provide a super smooth surface yielding a more perfect interface between the extruded shield and the insulation. LUTENE XL2808BK has stable volume resistivity characteristics at elevated temperatures and is formulated with a polymer system that has demonstrated compatibility with copper conductor.Applications: Insulation shielding of medium and high voltage cableInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D1505
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.8 MPa
2440 psi
ASTM D638
15.96 MPa

@Temperature 121 °C,
Time 605000 sec
2315 psi

@Temperature 250 °F,
Time 168 hour
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
207 %

@Temperature 121 °C,
Time 605000 sec
207 %

@Temperature 250 °F,
Time 168 hour
ASTM D638
Thermal Properties Metric English Comments
Melting Point 90.0 - 110 °C
194 - 230 °F
Electrical Properties Metric English Comments
Volume Resistivity 300 ohm-cm

@Temperature 23.0 °C
300 ohm-cm

@Temperature 73.4 °F
ASTM D257
800 ohm-cm

@Temperature 90.0 °C
800 ohm-cm

@Temperature 194 °F
ASTM D257
900 ohm-cm

@Temperature 135 °C
900 ohm-cm

@Temperature 275 °F
ASTM D257