Thermal Properties Metric English Comments
Melting Point 255 - 265 °C
491 - 509 °F
ASTM D789
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66)
The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah..
Melting Point 255 - 265 °C
491 - 509 °F
ASTM D789
PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66)
The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g..
Melting Point 238 - 265 °C
460 - 509 °F
Average value: 255 °C Grade Count:14
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Melting Point 254 - 265 °C
489 - 509 °F
Average value: 258 °C Grade Count:8
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Melting Point 254 - 265 °C
489 - 509 °F
Average value: 258 °C Grade Count:43
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Melting Point 221 - 265 °C
430 - 509 °F
Average value: 256 °C Grade Count:11
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Melting Point 255 - 265 °C
491 - 509 °F
Average value: 259 °C Grade Count:7
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Melting Point 254 - 265 °C
490 - 509 °F
Average value: 259 °C Grade Count:30
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Lucent Polymers 66-41 Nylon 66, Toughened
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Lucent Polymers G66-13 Nylon 66, 13% Glass Fiber Reinforced
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Lucent Polymers G66-33 Nylon 66, 33% Glass Fiber Reinforced
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Melting Point 255 - 265 °C
491 - 509 °F
ISO 3146-A
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 260 - 265 °C
500 - 509 °F
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Melting Point 215 - 265 °C
419 - 509 °F
Average value: 221 °C Grade Count:67
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Copyright © lookpolymers.com All Rights Reserved