Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ASTM D638
Elongation at Break >= 3.0 %
>= 3.0 %
ASTM D638
Flexural Strength 158.62 MPa
23006 psi
ASTM D790
Flexural Modulus 4.483 GPa
650.2 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.700 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 232.22 °C
450.00 °F
ASTM D648