Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 182 - 185 °C | 360 - 365 °F | |
Oceanchem Group Antioxidant 168 Molecular Formula: C42H63O3PCas No.: 31570-04-4Characteristics and Uses: This product is an excellent antioxidant namely applied to polyethylene, polypropylene, polyoxymethylene, ABS resin, PS resin.. |
|||
Melting Point | 182 - 193 °C | 360 - 379 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
Melting Point | 182 - 187 °C | 360 - 369 °F | Average value: 184 °C Grade Count:8 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 182 - 191 °C | 360 - 375 °F | |
Lucas-Milhaupt 60 Sn-40 Pb Tin/ Silver Solder Applications and Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is d.. |
|||
Melting Point | 182 °C | 360 °F | ASTM D2117 |
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang. |
|||
Melting Point | 182 °C | 360 °F | ISO 11357-1/-3 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Melting Point | 182 °C | 360 °F | ISO 11357-1/-3 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, dry Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Melting Point | 182 °C | 360 °F | By DSC |
Toyobo PELPRENE™ P55B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melting Point | 182 °C | 360 °F | By DSC |
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | 50% RH; DSC |
Suzhou Hipro Polymers Hiprolon® 211 ESNNHL P40 Nylon Hiprolon® 211ESNNHL P40 is a long chain polyamide compound from bio-renewable resource. It features low density, low water absorption, high dimension stability, high cold impact resistance, high bu.. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 182 °C | 360 °F | ASTM D789 |
Adell EZ-18 Homopolymer Polypropylene, 40% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |