| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.045 g/cc | 0.03775 lb/in³ | ASTM D792 |
| Water Absorption | 0.030 % | 0.030 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 50 | 50 | ASTM D785 |
| Hardness, Rockwell R | 78 | 78 | ASTM D785 |
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
| Elongation at Break | 80 % | 80 % | ASTM D638 |
| Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
| Flexural Modulus | 1.70 GPa | 247 ksi | ASTM D790 |
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
| Gardner Impact | 3.40 J | 2.51 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 182 °C | 360 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |