| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Water Absorption | 0.020 % | 0.020 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 62 | 62 | ASTM D785 |
| Hardness, Rockwell R | 90 | 90 | ASTM D785 |
| Tensile Strength, Ultimate | 35.2 MPa | 5110 psi | ASTM D638 |
| Elongation at Break | 6.0 % | 6.0 % | ASTM D638 |
| Flexural Strength | 50.3 MPa | 7300 psi | ASTM D790 |
| Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
| Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
| Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 182 °C | 360 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 127 °C | 261 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |