Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 134 °C | 273 °F | Internal method |
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er.. |
|||
Melting Point | 134 °C | 273 °F | Internal method |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Melting Point | 134 °C | 273 °F | Internal method |
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym.. |
|||
Melting Point | 134 °C | 273 °F | Internal method |
Polimeri Europa Eraclene® MQ 74 High Density Polyethylene - Injection Molding Eraclene MQ 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This resin is suggested in applications for which high creep, impact and st.. |
|||
Melting Point | 134 °C | 273 °F | Petromont |
Petromont 1000 High Density Polyethylene Resin Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to .. |
|||
Melting Point | 134 °C | 273 °F | Petromont |
Petromont 1002 High Density Polyethylene Resin Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl.. |
|||
Melting Point | 134 °C | 273 °F | Petromont |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Melting Point | 134 °C | 273 °F | |
LyondellBasell Lupolen® 5261 Z HDPE, Blow Molding Grade Relatively high viscosity blow molding grade for rigid, stackable and highly shock resistant containers for packaging all types of hazardous materials such as flammable, corrosive, poisonous and sur.. |
|||
Melting Point | 134 °C | 273 °F | ASTM D3418 |
LyondellBasell Microthene® F FA70000 High Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 134 °C | 273 °F | ASTM D3418 |
LyondellBasell Microthene® F FA70900 High Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 134 °C | 273 °F | ASTM D2117 |
Global B-5200 High Density Polyethylene Description-has excellent stiffness thus requires less material to make
blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global .. |
|||
Melting Point | 134 °C | 273 °F | ASTM D2117 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Melting Point | 134 °C | 273 °F | DSC |
LG Chemical LUTENE-H BE0350 HDPE Description: LUTENE-H BE0350 is an excellent material for blow-molded articles with high density and rigidity. It has good flow characteristics, high parison stability and impact resistance.Applicat.. |
|||
Melting Point | 134 - 181 °C | 273 - 358 °F | |
Indium Corp. Indalloy 5 Indium-Lead-Tin Solder Alloy Very good resistance to alkaline corrosionInformation Provided by Indium Corporation |
|||
Melting Point | 134 °C | 273 °F | ASTM D2117 |
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Melting Point | 134 °C | 273 °F | ISO 11357 |
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M5510 EP is a second generation metallocene high density homopolymer polyethylene.Lumicene® mPE M5510 EP can be processed at high output ra.. |
|||
Melting Point | 134 °C | 273 °F | ISO 11357 |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Melting Point | 134 - 181 °C | 273 - 358 °F | |
Williams Advanced Alloys WS181 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 134 °C | 273 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® E100 Polymer Modifier DuPont™ Fusabond® E100 is an anhydride modified high density polyethylene, mainly intended for use as a component in a blend with other polymers including polyolefins and polyamides. It is not int.. |
|||
Melting Point | 134 °C | 273 °F | Dow Method (DSC) |
Dow DS6D81 Polypropylene Resin DOW DS6D81 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Melting Point | 134 °C | 273 °F | DSC; Dow Method |
Dow DS6D82 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D82 Polypropylene Resin is intended for use as a heat seal coati.. |
|||
Melting Point | 134 °C | 273 °F | Dow Method (DSC) |
Dow DS6D82 Polypropylene Resin DOW DS6D82 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Melting Point | 134 °C | 273 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |
|||
Melting Point | 134 °C | 273 °F | DSC |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Melting Point | 134 °C | 273 °F | DSC |
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip.. |
|||
Melting Point | 134 °C | 273 °F | DSC |
Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Melting Point | 134 °C | 273 °F | ISO 11357 |
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Melting Point | 134 °C | 273 °F | ISO 11357 |
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor.. |
|||
Melting Point | 134 °C | 273 °F | Peak; ExxonMobil Method |
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupli.. |
|||
Melting Point | 134 - 204 °C | 272 - 399 °F | Average value: 161 °C Grade Count:80 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |